RA 6Al-2Sn-4Zr-2Mo
Sheet & Strip under 0.1875" thickness: Duplex anneal: 1650 ± 25°F), 30± 3 minutes, air cool, followed by 1450± 25°F 15± 2 minutes, air cool. Triplex anneal: 1650°F ½ hour, air cool, followed by 1450°F ¼ hour, air cool, 1100°F 2 hours air cool.
Plate 0.1875 inch thickness and over: Duplex anneal: 650± 25°F 60± 5 minutes, air cool, followed by 1100±25°F 8 hours ± 15 minutes, air cool. Triplex anneal: 1650°F ½ hour, air cool, followed by 1450°F ¼, air cool, 1100°F 2 hours air cool.
Bar and Forgings: Duplex anneal: Solution anneal 25 - 50°F below. Beta transus 1 hour, air cool or faster, 1100°F 8 hours air cool.