Alloy 17-4PH (UNS S17400), Type 630, is a chromium-nickel-copper precipitation-hardening martensitic stainless steel with an addition of niobium. 17-4PH combines high strength and hardness with good corrosion resistance.

The alloy is furnished in the solution annealed condition (Condition A). It should not be used at temperatures above 572°F (300°C) or for cryogenic service. Optimal mechanical properties can be obtained by subjecting the alloy to age hardening heat treatments. Heat treatment in the 900°F (482°C) range produces the highest strength.

The corrosion resistance of Alloy 17-4PH is comparable to 304 stainless steel in most environments, and is generally superior to the 400 series stainless steels. It is used in applications where the combination of moderate corrosion resistance and unusually high strength are required.

Alloy 17-4PH can be easily welded and processed by standard shop fabrication practices. It is magnetic.

Applications
  • Aerospace — structural and parts
  • Biomedical — hand tools
  • Chemical Processing
  • Food Process Equipment
  • Gate Valves
  • Mechanical Components
  • Nuclear Waste Processing and Storage
  • Oil and Gas Production — foils, helicopter deck platforms, etc.
  • Pulp and Paper — paper mill equipment
总览  
材料状态 
  • 已商用:当前有效
供货地区 
  • 亚太地区
  • 北美洲
  • 拉丁美洲
  • 欧洲
  • 非洲和中东
Available Documents
Technical Datasheet (English)
Metals General
额定值
单位制
 
Applicable Specifications
 
 
Forms Available
 
 
Metal Type
 
 
Alloy Identification
 
 
Metals Type Analysis
额定值
单位制
 
Type Analysis
     
Carbon
%
 
Chromium
%
 
Copper
%
 
Iron (Balance)
%
 
Manganese
%
 
Nickel
%
 
Niobium + Tantalum
%
 
Phosphorus
%
 
Silicon
%
 
Sulfur
%
 
Metals Physical
额定值
单位制
 
密度
lb/in³
 
Metals Mechanical
额定值
单位制
 
Tensile Strength (Ultimate) 2
ksi
 
Tensile Strength (Yield), 0.2% 2
ksi
 
Tensile Elongation (Break) 2
%
 
Reduction of Area 2
%
 
硬度 2 (HRC-Scale)
 
 
拉伸模量
ksi
 
Metals Thermal
额定值
单位制
 
Mean Specific Heat (68°F)
Btu/lb/°F
 
Mean CTE (70 到 801°F)
in/in/°F
 
导热系数 (212°F)
Btu·in/hr/ft²/°F
 
Metals Electrical
额定值
单位制
 
Electrical Resistivity (75°F)
ohms·cir·mil/ft
 
备注
1一般属性:这些不能被视为规格。
2Condition: H900
 
UL 和 UL 徽标为 UL LLC © 的商标 2022。保留所有权利。
此数据表中的信息由 UL Prospector 从该材料的生产商处获得。UL Prospector 尽最大努力确保此数据的准确性。 但是 UL Prospector 对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。