Sandmeyer Stainless Steel Alloy 347H 数据表

Wrought Stainless Steel

用Sandmeyer Steel Company提供

Create your free Prospector account to view this complete product datasheet. A free account includes access to hundreds of thousands of detailed technical datasheets. 创建您的免费帐号
产品说明
Alloy 347 (UNS S34700) is a columbium stabilized austenitic stainless steel with good general corrosion resistance and somewhat better resistance in strong oxidizing conditions than 321 (UNS S32100). It has excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 - 1500°F (427 - 816°C). The alloy has good oxidation resistance and creep strength to 1500°F (816°C). It also possesses good low temperature toughness.

Alloy 347H (UNS S3409) is the higher carbon (0.04 - 0.10) version of the alloy. It was developed for enhanced creep resistance and for higher strength at temperatures above 1000°F (537°C). In most instances, the carbon content of the plate enables dual certification.

Alloy 347 cannot be hardened by heat treatment, only by cold working. It can be easily welded and processed by standard shop fabrication practices.

Applications
  • Chemical Processing
  • Food Processing - equipment and storage
  • Petroleum Refining - fluid catalytic cracking units, polythionic acid service
  • Waste Heat Recovery - recuperators
总览  
材料状态 
  • 已商用:当前有效
供货地区 
  • 亚太地区
  • 北美洲
  • 拉丁美洲
  • 欧洲
  • 非洲和中东
Available Documents
Technical Datasheet (English)
Metals General
额定值
单位制
 
Applicable Specifications
 
 
Forms Available
 
 
Metal Type
 
 
Alloy Identification
 
 
Metals Type Analysis
额定值
单位制
 
Type Analysis
     
Carbon
%
 
Chromium
%
 
Columbium + Tantalum
%
 
Iron (Balance)
%
 
Manganese
%
 
Nickel
%
 
Phosphorus
%
 
Silicon
%
 
Sulfur
%
 
Metals Physical
额定值
单位制
 
密度
lb/in³
 
Metals Mechanical
额定值
单位制
 
Tensile Strength (Ultimate)
ksi
 
Tensile Strength (Yield), 0.2%
ksi
 
Tensile Elongation (Break)
%
 
硬度 (HB-Scale)
 
 
拉伸模量
ksi
 
Metals Thermal
额定值
单位制
 
Mean Specific Heat (32 到 212°F)
Btu/lb/°F
 
Mean CTE (68 到 212°F)
in/in/°F
 
导热系数 (212°F)
Btu·in/hr/ft²/°F
 
Metals Electrical
额定值
单位制
 
Electrical Resistivity (68°F)
ohms·cir·mil/ft
 
备注
1一般属性:这些不能被视为规格。
 
UL 和 UL 徽标为 UL LLC © 的商标 2022。保留所有权利。