HARRIS® BLOCKADE®
Blockade is an excellent choice for brass brazing. Its low melting point reduces the likelihood of overheating the brass. It is often selected to replace high silver brazing filler metals for these applications. Blockade does not contain silver so significant cost reductions are available.
Blockade is not recommended for brazing steel or other ferrous alloys. The phosphorus content will form a low ductility intermetallic with the base metal. Phosphorus containing brazing alloys should not be used if the braze is exposed to sulfur or sulfur compounds in service.
AVAILABLE FORMS
Standard wire diameters in coils and rod. Preform rings
RECOMMENDED FLUX:
No flux is required for copper brazing. For brazing brass or copper to brass, use Stay-Silv ® white flux.
一般属性
使用 Prospector 建立免費帳戶時,可造訪 HARRIS® BLOCKADE® 的完整資料表詳細資訊。您將找到有關物理、機械和硬度規格的完整資訊
Technical Datasheet (English)
下载文档加工
Find specific processing information for HARRIS® as well as general information for the Copper - Wrought - Phosphor Bronze generic family. 注册 或 登录 了解更多信息。