产品说明 | ||||
SM25CR is a Duplex Stainless Steel material, generically called Duplex due to its dual micro structure composed of approximately 50% Ferrite and 50% Austenite. SM25CR is used in corrosive well conditions in combined presence of CO2, low H2S and Chlorides, where material strength is also required.
Launched in the early 80's, SM25CR benefits from NSSMC's unrivaled know-how in manufacturing CRA (Corrosion Resistance Alloys) materials and best-in-class quality control. SM25CR-125 is manufactured based on API 5CT/ISO 11960 and API 5CRA/ISO 13680. |
||||
总览 | ||||
材料状态
|
|
|||
供货地区
|
|
Available Documents | |||
Technical Datasheet (English)
|
|||
Metals General |
额定值
|
单位制
|
|
Forms Available
|
|
|
|
Metal Type
|
|
|
|
Alloy Identification
|
|
|
|
Metals Type Analysis |
额定值
|
单位制
|
|
Type Analysis
|
|||
Carbon
|
|
%
|
|
Chromium
|
|
%
|
|
Copper
|
|
%
|
|
Manganese
|
|
%
|
|
Molybdenum
|
|
%
|
|
Nickel
|
|
%
|
|
Nitrogen
|
|
%
|
|
Silicon
|
|
%
|
|
Tungsten
|
|
%
|
|
Metals Physical |
额定值
|
单位制
|
|
密度 (77°F)
|
|
lb/in³
|
|
Metals Mechanical |
额定值
|
单位制
|
|
Tensile Strength (Ultimate)
|
|
ksi
|
|
Tensile Strength (Yield), 0.2%
|
|
ksi
|
|
Tensile Elongation (Yield)
|
|
%
|
|
硬度 (HRC-Scale)
|
|
|
|
泊松比 (77°F)
|
|
|
|
拉伸模量 (77°F)
|
|
ksi
|
|
Metals Thermal |
额定值
|
单位制
|
|
Mean Specific Heat (77°F)
|
|
Btu/lb/°F
|
|
Mean CTE (212°F)
|
|
in/in/°F
|
|
导热系数 (77°F)
|
|
Btu·in/hr/ft²/°F
|
|
Thermal Diffusivity (77°F)
|
|
in²/s
|
备注 |
1一般属性:这些不能被视为规格。 |
UL 和 UL 徽标为 UL LLC © 的商标 2021。保留所有权利。
此数据表中的信息由 UL Prospector 从该材料的生产商处获得。UL Prospector 尽最大努力确保此数据的准确性。 但是 UL Prospector 对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |