产品说明 | ||||
Increased Carbon, Molybdenum and Nickel over basic die steel compositions offer enhanced abrasion resistance and good impact toughness for the following applications.
Aluminum and Titanium Forging Appropriate for hammer forging of aluminum where strain rates and the formation of abrasive aluminum-oxide exert strong wear forces on the die. Warm (Ferrous) Forging Forging steel at lower temperatures offers improved dimensional precision and improved heating efficiency, but subjects the dies to increased cavity pressures and strong abrasion forces. Water quenched DURODI offers excellent performance under these conditions through a balanced combination of enhanced wear resistance and good impact toughness. Counterblow Hammers Large counterblow hammer dies are subjected to incredibly high impact forces and flow stresses. The combination of cold-water quenching and the deep hardening capacity of DURODI provide the microstructure and hardness needed for large counterblow hammer dies. Machinability Machinability at all hardness levels is enhanced through patented micro-alloying additions, but where maximum machinability is desired, a fully annealed condition (approximately 248 HB) is available. |
||||
总览 | ||||
材料状态
|
|
|||
供货地区
|
|
Available Documents | |||
Technical Datasheet (English)
|
|||
Metals General |
额定值
|
单位制
|
|
Metal Type
|
|
|
|
Metals Type Analysis |
额定值
|
单位制
|
|
Type Analysis
|
|||
Carbon
|
|
%
|
|
Chromium
|
|
%
|
|
Manganese
|
|
%
|
|
Molybdenum
|
|
%
|
|
Nickel
|
|
%
|
|
Silicon
|
|
%
|
|
Vanadium
|
|
%
|
|
Metals Physical |
额定值
|
单位制
|
|
密度 (68°F)
|
|
lb/in³
|
|
Metals Mechanical |
额定值
|
单位制
|
|
泊松比 (68°F)
|
|
|
|
拉伸模量 (68°F)
|
|
ksi
|
|
Metals Thermal |
额定值
|
单位制
|
|
Mean Specific Heat (68°F)
|
|
Btu/lb/°F
|
|
Mean CTE (68°F)
|
|
in/in/°F
|
|
导热系数 (68°F)
|
|
Btu·in/hr/ft²/°F
|
备注 |
1一般属性:这些不能被视为规格。 |
UL 和 UL 徽标为 UL LLC © 的商标 2021。保留所有权利。