Outokumpu 353 MA®
All steels except EN 1.4948 (i.e., all EN 1.48XX) are included in the European Standard EN 10095 "Heat-resisting steels and nickel alloys". EN 1.4948 is included in EN 10028-7 "Flat products made of steels for pressure purposes - Part 7: Stainless steel". All the above steel grades are also included in ASTM A240.
353 MA® is an alloy with a significantly higher nickel content than the other steels. Like 153 MA™ and 253 MA® it has increased contents of silicon and nitrogen, and is microalloyed with rare earth metals (REM). The maximum service temperature in air is 1150°C, but after service at temperatures below ~950°C there is a risk for reduced room temperature impact toughness.