TIMETAL 75A is equivalent to ASTM Grade 4. It has the highest str ength of the four ASTM commercially pure titanium grades in addition to good ductility and moderate formability. The benefits of the good strength to weight ratio of TIMETAL 75A are retained at moderate temperatures. TIMETAL 75A is typically used in continuous service up to 800°F (425°C) and in intermittent service up to 1000°F (540°C). It also has good impact properties at low temperatures. In addition, TIMETAL 75A can be satisfactorily welded, machined, cold worked, hot worked, and cast.
总览  
材料状态 
  • 已商用:当前有效
供货地区 
  • 北美洲
  • 欧洲
  • 亚太地区
Available Documents
Technical Datasheet (English)
Metals General
额定值
单位制
 
Forms Available
 
 
Metal Type
 
 
Metals Type Analysis
额定值
单位制
 
Type Analysis
     
Carbon
%
 
Hydrogen
%
 
Iron
%
 
Nitrogen
%
 
Other Elements
%
 
Oxygen
%
 
Titanium
%
 
Metals Physical
额定值
单位制
 
密度
lb/in³
 
Metals Mechanical
额定值
单位制
 
Tensile Strength (Ultimate)
ksi
 
Tensile Strength (Yield), 0.2%
ksi
 
Tensile Elongation (Break)
%
 
Reduction of Area
%
 
拉伸模量 (68 到 78°F)
ksi
 
Metals Thermal
额定值
单位制
 
Mean CTE (68 到 212°F)
in/in/°F
 
导热系数
Btu·in/hr/ft²/°F
 
Metals Electrical
额定值
单位制
 
Electrical Resistivity