HARRIS® GAL-VIV
PROCEDURE:
Remove all rust, slag and other foreign material from the area to be galvanized. No flux is needed for this process. The base metal must be heated to approximately 600°F (315°C). Rub the rod on the area to be coated, letting the heat from the base metal melt the rod. Do not apply torch directly onto the Gal-viz. Thinning action can be improved by brushing through the molten deposit using a clean wire brush. The alloy can be smoothed out with a paddle or cloth; DO NOT OVERHEAT! This product is intended to be used in the flat position, vertical is not recommended and overhead should never be performed.