ATI Steel ATI 348™
While ATI 321, ATI 347 and ATI 348 alloy continue to be employed for prolonged service in the 800 to 1500°F (427 to 816°C) temperature range, ATI 304L™alloy has supplanted these stabilized grades for applications involving only welding or short time heating. (For information on ATI 304L alloy, consult the Technical Data Sheet for ATI 304L™ alloy.)
ATI 321, ATI 347 and ATI 348 stainless steels are also advantageous for high temperature service because of their good mechanical properties. ATI 321, ATI 347 and ATI 348 stainless steels offer higher creep and stress rupture properties than ATI 304 alloy and, particularly, ATI 304L stainless which might also be considered for exposures where sensitization and intergranular corrosion are concerns. This results in higher elevated temperature allowable stresses for these stabilized alloys for ASME Boiler and Pressure Vessel Code applications. The ATI 321, ATI 347 and ATI 348 alloys have maximum use temperatures of 1500°F (816°C) for code applications as does ATI 304™ stainless, whereas ATI T304L™stainless is limited to 800°F (426°C).
The properties of ATI 348 stainless are similar to the properties of ATI 347 alloy, and according to ASTM A240 their chemical compositions are the same except for tantalum and cobalt contents.
High carbon versions of all three alloys are available. These grades have UNS designations S32109, S34709, and S34809.
一般属性
使用 Prospector 建立免費帳戶時,可造訪 ATI Steel ATI 348™ 的完整資料表詳細資訊。您將找到有關物理、機械和硬度規格的完整資訊
Technical Datasheet (English)
下载文档加工
Find specific processing information for ATI Steel as well as general information for the Steel - Wrought - Stainless - Austenitic generic family. 注册 或 登录 了解更多信息。