CarTech® Pyrotool® Alloy 7
To achieve the best combination of hardness and toughness for tooling applications, CarTech Pyrotool alloy 7 is annealed and solution treated simultaneously at 1750°F (954°C) for one hour, then air cooled. It is then aged at 1325°F (718°C) for eight hours, slow cooled 100°F (38°C) per hour to 1150°F (621°C), held for eight hours and air cooled.
CarTech Pyrotool alloy 7, when aged, attains a hardness of Rockwell C 40/44.