Outokumpu 4713
The two lower alloyed grades are best suited for temperatures between 550°C and 850°C, at which most HT austenitic stainless steels are prone to form brittle phases. The higher alloyed ones are applied at temperatures up to 1150°C and show excellent resistance against reducing sulphur attacks and molten metals.
Due to their ferritic structure, the ferritic steels show lower strength at temperatures exceeding 600°C, but are more resistant to thermal shocks than HT austenitic stainless steels. With the thermal conductivity higher and the thermal expansion lower than the respective values for austenitic steels, equal thermal shocks will result in lower thermal stresses in the ferritic material. In these terms, ferrites allow greater tolerances for design and operation.
All grades are included in the European Standard EN 10095 "Heat-resisting steels and nickel alloys".
4713 does not form brittle phases but should only be exposed to moderately corrosive atmospheres owing to its low chromium content.
Propriedades gerais
Acesse os detalhes completos da ficha de dados de Outokumpu 4713 quando você criar sua conta gratuita no Prospector. Você encontrará informações completas sobre especificações físicas, mecânicas e de dureza
Technical Datasheet (English)
Baixar o documentoProcessamento
Encontre informações de processamento específicas para Outokumpu, além de informações gerais para a família genérica Steel - Wrought - Stainless - Ferritic. Inscreva-se ou Faça login para mais informações.
Onde comprar
Você pode adquirir Outokumpu 4713 de 1 distribuidores ou fabricantes. Inscreva-se ou Faça login para mais informações.
PROSPECTOR
Encontre soluções, não somente materiais.
Quando se junta ao Prospector, você se beneficia de recursos e ferramentas dinâmicas para encontrar soluções rapidamente..
Inscreva-se hoje mesmo