RA 6Al-4V

ジェネリックファミリー: Titanium - Wrought - Alpha-Beta Alloy提供元: Rolled Alloys
Ti 6Al-4V is the most widely used of all the alpha-beta titanium alloys. It is typically used in the annealed condition, at service temperatures through 750°F. However it may be heat treated for high strength in sections under 4" thick. Hardenability is limited and sections over one inch may not develop full properties. Ti 6Al-4V is welded with either matching or ELI (Extra Low Interstitials) filler wire.

Mill anneal: 1300-1450°F 2 hours, air cool. Recrystallization anneal bar for better ductility and fatigue strength, 1750°F 2 hours, furnace cool. For maximum fracture toughness and SCC resistance: Beta anneal 1950°F 1-2 hours, water quench. Then age 1150-1300°F 2 to 4 hours, air cool. For maximum strength: solution-treated and aged (STA) condition is: For sheet, 1675-1725°F 5 to 25 minutes, water quench. Age 975°F 4 to 6 hours, air cool. For bars and forgings, 1675-1725°F 1 hour, water quench. Age 975-1025°F 3 hours, air cool. For increased fracture toughness, but lower tensile strength: precipitation treat (overage) 1150-1250°F 4 hours, air cool. Stress relief: annealing is commonly 1000-1200°F 1 to 4 hours, air cool.

Ti 6Al-4V is resistant to general corrosion but may be quickly attacked by environments that cause breakdown of the protective oxide. These include hydrofluoric (HF), hydrochloric (HCl), sulfuric and phosphoric acids. Inhibitors may help for the last four but not for HF. Ti 6Al-4V resists attack by pure hydrocarbons, and most chlorinated and fluorinated hydrocarbons (provided water has not caused formation of small amounts of HCl and HF).

Ti 6Al-4V is susceptible to chloride stress corrosion cracking (SCC), although being among the better of the titanium alloys in this regard. For marine environments silver plated bolts are not used, as silver bonds easily with chlorine in this environment. Ti 6Al-4V is also susceptible to SCC in environments such as methyl alcohol, red fuming HNO3, and N2O4. In the case of red fuming nitric acid, the problem is limited to environments containing less than 1.5% water, or more than 6% NO2. Failure in N2O4 has occurred when oxygen and chlorides were present as impurities.
一般的な属性

Prospectorで無料のアカウントを作成し、RA 6Al-4Vのデータシート詳細すべてにアクセスします。そこで、物理、機械、硬度仕様に関するすべての情報をご覧ください

材料ステータス
供給可能
ドキュメント
description

Technical Datasheet (English)

ドキュメントのダウンロード
可用性
アジア太平洋地域, 欧州, 北アメリカ
その他の属性
Applicable Specifications, Metal Type, Alloy Identification, Type Analysis, 密度, Tensile Strength (Ultimate), Tensile Strength (Yield), 0.2%, Tensile Elongation (Break), Reduction of Area, 引張係数, Mean CTE, 熱伝導性
Access 12 properties in Metals. Create your free account or sign into Prospector.
加工

RAの具体的な加工情報や、Titanium - Wrought - Alpha-Beta Alloyジェネリックファミリーの一般情報をご確認いただけます。 登録 または サインイン 詳細情報を確認してください。

ご購入方法

1の販売業者や製造者からRA 6Al-4Vを購入できます。 登録 または サインイン 詳細情報を確認してください。

Prospectorのログイン/登録
プレミアム機能

PROSPECTOR

材料だけでなく、ソリューションも見つけることができます。

Prospectorにご登録いただくと、ダイナミックなツールおよび機能を活用して、迅速にソリューションを見つけることができます。

今すぐご登録ください