ジェネリックファミリー: Zirconium - Wrought - Alloy提供元: Allegheny Technologies Incorporated
Zircadyne® alloys are composed of 95.5% to 99.2% zirconium and hafnium with a maximum hafnium content of 4.5%. Zircadyne mill products are available in two chemical grades each sharing excellent corrosion resistance and also having slightly different physical and mechanical properties. Zircadyne 702 Zirconium is commercially pure. Zircadyne 705 zirconium is alloyed with niobium to increase its strength and improve its formability. Table 1 shows the chemical composition of Zircadyne alloys. The presence of hafnium in Zircadyne alloys does not significantly influence the physical, mechanical, or corrosion properties.

Zirconium, a reactive metal, has a high affinity for oxygen that results in the formation of a protective oxide layer in air at room temperature. This protective oxide gives Zircadyne alloys their superior corrosion resistance and this oxide layer can be enhanced through a heat treating process. A properly formed enhanced oxide layer serves as an excellent bearing surface against a variety of materials, imparts impressive erosion resistance in high velocity systems, and can improve the corrosion resistance in certain aggressive environments.

Zircadyne alloys exhibit good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys. In addition to being integral to the oxide layer, oxygen is an interstitial strengthening element in Zircadyne alloys. Zircadyne alloys do not exhibit a low temperature ductile to brittle transition.
一般的な属性

Prospectorで無料のアカウントを作成し、ATI Zirconium ATI Zircadyne® 702のデータシート詳細すべてにアクセスします。そこで、物理、機械、硬度仕様に関するすべての情報をご覧ください

材料ステータス
供給可能
ドキュメント
description

Technical Datasheet (English)

ドキュメントのダウンロード
可用性
アジア太平洋地域, アフリカ&中東, ラテンアメリカ, 欧州, 北アメリカ
その他の属性
Forms Available, Metal Type, Alloy Identification, Type Analysis, 密度, Tensile Strength (Ultimate), Tensile Strength (Yield), 0.2%, Tensile Elongation (Break), ポアゾン比, 引張係数, 弾性係数, Mean Specific Heat, Mean CTE, 熱伝導性
Access 14 properties in Metals. Create your free account or sign into Prospector.
加工

ATI Zirconiumの具体的な加工情報や、Zirconium - Wrought - Alloyジェネリックファミリーの一般情報をご確認いただけます。 登録 または サインイン 詳細情報を確認してください。

ご購入方法

1の販売業者や製造者からATI Zirconium ATI Zircadyne® 702を購入できます。 登録 または サインイン 詳細情報を確認してください。

Prospectorのログイン/登録
プレミアム機能

PROSPECTOR

材料だけでなく、ソリューションも見つけることができます。

Prospectorにご登録いただくと、ダイナミックなツールおよび機能を活用して、迅速にソリューションを見つけることができます。

今すぐご登録ください