ATI Steel ATI 15-5™
The ATI 15-5™ alloy was designed to have greater toughness than S17400, especially in the through-thickness (short transverse) direction. This improved toughness is achieved by reduced delta ferrite content and control of inclusion size and shape. The composition and processing of ATI 15-5™ alloy is carefully controlled to minimize its content of delta ferrite, which is present in the S17400 material. Inclusion control is done by consumable electrode remelting using the electro-slag remelting (ESR) process.
The S15500 alloy is martensitic in structure in the annealed condition and is further strengthened by a relatively low temperature heat treatment, which precipitates a copper containing phase in the alloy. Like the S17400 alloy, the S15500 alloy requires only a simple heat treatment; a one-step process conducted at a temperature in the range 900°F (482°C) to 1150°F (621°C) depending on the combination of strength and toughness desired.
A wide range of properties can be produced by this one-step heat treatment. Heat treatment in the 900°F (482°C) range produces the highest strength, although it is slightly less than those of semi-austenitic alloys like S17700 or S15700. The latter precipitation hardening stainless steels generally require more steps to complete heat treatment. The ATI 15-5™ alloy is generally better suited for plate applications than are the semiaustenitic alloys.
一般的な属性
Prospectorで無料のアカウントを作成し、ATI Steel ATI 15-5™のデータシート詳細すべてにアクセスします。そこで、物理、機械、硬度仕様に関するすべての情報をご覧ください
Technical Datasheet (English)
ドキュメントのダウンロード加工
ATI Steelの具体的な加工情報や、Steel - Wrought - Stainless - Precipitation Hardeningジェネリックファミリーの一般情報をご確認いただけます。 登録 または サインイン 詳細情報を確認してください。
ご購入方法
1の販売業者や製造者からATI Steel ATI 15-5™を購入できます。 登録 または サインイン 詳細情報を確認してください。
PROSPECTOR
材料だけでなく、ソリューションも見つけることができます。
Prospectorにご登録いただくと、ダイナミックなツールおよび機能を活用して、迅速にソリューションを見つけることができます。
今すぐご登録ください