RA 6Al-2Sn-4Zr-2Mo
Sheet & Strip under 0.1875" thickness: Duplex anneal: 1650 ± 25°F), 30± 3 minutes, air cool, followed by 1450± 25°F 15± 2 minutes, air cool. Triplex anneal: 1650°F ½ hour, air cool, followed by 1450°F ¼ hour, air cool, 1100°F 2 hours air cool.
Plate 0.1875 inch thickness and over: Duplex anneal: 650± 25°F 60± 5 minutes, air cool, followed by 1100±25°F 8 hours ± 15 minutes, air cool. Triplex anneal: 1650°F ½ hour, air cool, followed by 1450°F ¼, air cool, 1100°F 2 hours air cool.
Bar and Forgings: Duplex anneal: Solution anneal 25 - 50°F below. Beta transus 1 hour, air cool or faster, 1100°F 8 hours air cool.
Propriétés générales
Consultez la fiche technique complète de RA 6Al-2Sn-4Zr-2Mo en créant gratuitement votre compte Prospector. Vous y trouverez des informations exhaustives sur les propriétés physiques et mécaniques et sur la dureté
Technical Datasheet (English)
Télécharger le documentTraitement en cours
Find specific processing information for RA as well as general information for the Titanium - Wrought - Alpha Alloy generic family. S’inscrire ou Connexion pour en savoir plus.
Où acheter
Vous pouvez acheter RA 6Al-2Sn-4Zr-2Mo auprès de 1 distributeurs ou fabricants. S’inscrire ou Connexion pour en savoir plus.