Kanthal® Thermocouple Iron
The alloy is transformed magnetically at 770°C (1420°F) and a crystallographic transformation occurs at 900°C (1650°F). Both transformations affect the thermoelectric properties of the alloy.
Iron can not be exposed to sulphur-containing atmospheres and to temperatures below zero. Thermocouple iron wire is supplied copper-coated to prevent oxidation.
Thermocouple type J and L are frequently used because of their high emf output and their low cost. Compensating cables of type KCA are used together with thermocouples of type K.
Propriétés générales
Consultez la fiche technique complète de Kanthal® Thermocouple Iron en créant gratuitement votre compte Prospector. Vous y trouverez des informations exhaustives sur les propriétés physiques et mécaniques et sur la dureté
Technical Datasheet (English)
Télécharger le documentTraitement en cours
Find specific processing information for Kanthal® as well as general information for the Iron - Wrought - Commercially Pure generic family. S’inscrire ou Connexion pour en savoir plus.
Où acheter
Vous pouvez acheter Kanthal® Thermocouple Iron auprès de 1 distributeurs ou fabricants. S’inscrire ou Connexion pour en savoir plus.
PROSPECTOR
Trouvez des solutions, pas seulement des matériaux..
Avec Prospector, vous disposez d’outils et de fonctions dynamiques qui vous permettront de trouver des solutions au plus vite.
S’inscrire aujourd’hui