Outokumpu 4713
The two lower alloyed grades are best suited for temperatures between 550°C and 850°C, at which most HT austenitic stainless steels are prone to form brittle phases. The higher alloyed ones are applied at temperatures up to 1150°C and show excellent resistance against reducing sulphur attacks and molten metals.
Due to their ferritic structure, the ferritic steels show lower strength at temperatures exceeding 600°C, but are more resistant to thermal shocks than HT austenitic stainless steels. With the thermal conductivity higher and the thermal expansion lower than the respective values for austenitic steels, equal thermal shocks will result in lower thermal stresses in the ferritic material. In these terms, ferrites allow greater tolerances for design and operation.
All grades are included in the European Standard EN 10095 "Heat-resisting steels and nickel alloys".
4713 does not form brittle phases but should only be exposed to moderately corrosive atmospheres owing to its low chromium content.
Propiedades generales
Acceda a los detalles completos de la hoja de datos de Outokumpu 4713 cuando cree su cuenta gratuita con Prospector. Encontrará información completa sobre especificaciones físicas, mecánicas y de dureza
Technical Datasheet (English)
Descargar documentoProcesando
Encuentre información de procesamiento específica para Outokumpu, así como información general para la familia genérica de Steel - Wrought - Stainless - Ferritic. Registrarse o Iniciar sesión para obtener más información.
Dónde comprar
Puede comprar Outokumpu 4713 de 1 distribuidores o fabricantes. Registrarse o Iniciar sesión para obtener más información.
PROSPECTOR
Encuentre soluciones, no solo materiales.
Cuando se une a Prospector, aprovecha las herramientas y funciones dinámicas para encontrar soluciones rápidamente.
Regístrese hoy