RA 6Al-2Sn-4Zr-2Mo
Sheet & Strip under 0.1875" thickness: Duplex anneal: 1650 ± 25°F), 30± 3 minutes, air cool, followed by 1450± 25°F 15± 2 minutes, air cool. Triplex anneal: 1650°F ½ hour, air cool, followed by 1450°F ¼ hour, air cool, 1100°F 2 hours air cool.
Plate 0.1875 inch thickness and over: Duplex anneal: 650± 25°F 60± 5 minutes, air cool, followed by 1100±25°F 8 hours ± 15 minutes, air cool. Triplex anneal: 1650°F ½ hour, air cool, followed by 1450°F ¼, air cool, 1100°F 2 hours air cool.
Bar and Forgings: Duplex anneal: Solution anneal 25 - 50°F below. Beta transus 1 hour, air cool or faster, 1100°F 8 hours air cool.
General Properties
Access the complete datasheet details for RA 6Al-2Sn-4Zr-2Mo when you create your free account with Prospector. You’ll find complete information on physical, mechanical and hardness specs.
Technical Datasheet (English)
Download DocumentProcessing
Find specific processing information for RA as well as general information for the Titanium - Wrought - Alpha Alloy generic family. Register or Sign In for more information.
Where To Buy
You can purchase RA 6Al-2Sn-4Zr-2Mo from 1 distributors or manufacturers. Register or Sign In for more information.
PROSPECTOR
Find solutions, not just materials.
When you join Prospector, you leverage the dynamic tools and features to find solutions fast.
Register Today