CarTech® Pyrotool® Alloy 7
To achieve the best combination of hardness and toughness for tooling applications, CarTech Pyrotool alloy 7 is annealed and solution treated simultaneously at 1750°F (954°C) for one hour, then air cooled. It is then aged at 1325°F (718°C) for eight hours, slow cooled 100°F (38°C) per hour to 1150°F (621°C), held for eight hours and air cooled.
CarTech Pyrotool alloy 7, when aged, attains a hardness of Rockwell C 40/44.
Applications:
Key uses for this grade have been:
High-temperature tooling
Extrusion dies
Forging dies
Rams
Mandrels
Holders
Rings
Dummy blocks
Liners
General Properties
Access the complete datasheet details for CarTech® Pyrotool® Alloy 7 when you create your free account with Prospector. You’ll find complete information on physical, mechanical and hardness specs.
Technical Datasheet
Download DocumentProcessing
Find specific processing information for CarTech® as well as general information for the Steel - Wrought - Tool Steel generic family. Register or Sign In for more information.
Where To Buy
You can purchase CarTech® Pyrotool® Alloy 7 from 1 distributors or manufacturers. Register or Sign In for more information.
PROSPECTOR
Find solutions, not just materials.
When you join Prospector, you leverage the dynamic tools and features to find solutions fast.
Register Today