Outokumpu 4762
The two lower alloyed grades are best suited for temperatures between 550°C and 850°C, at which most HT austenitic stainless steels are prone to form brittle phases. The higher alloyed ones are applied at temperatures up to 1150°C and show excellent resistance against reducing sulphur attacks and molten metals.
Due to their ferritic structure, the ferritic steels show lower strength at temperatures exceeding 600°C, but are more resistant to thermal shocks than HT austenitic stainless steels. With the thermal conductivity higher and the thermal expansion lower than the respective values for austenitic steels, equal thermal shocks will result in lower thermal stresses in the ferritic material. In these terms, ferrites allow greater tolerances for design and operation.
4762 - with the highest chromium content- is the most resistant to reducing sulphurous gases. It is susceptible to the same embrittlement phenomena as 4742 whilst s-phase forms during long exposures in the range 600°C to 800°C.
Allgemeine Eigenschaften
Richten Sie ein kostenloses Prospector-Konto ein, um Zugang zu sämtlichen Angaben des Produktdatenblatts von Outokumpu 4762 zu erhalten. Dort finden Sie alle Angaben zu den physikalischen, mechanischen und Härteeigenschaften
Technical Datasheet (English)
Dokument herunterladenVerarbeitung
Finden Sie bestimmte Informationen zur Verarbeitung für Outokumpu sowie allgemeine Informationen zum allgemeinen Produktkreis Steel - Wrought - Stainless - Ferritic. Registrieren oder Anmelden um mehr Informationen erhalten.
Bezugsquellen
Sie können Outokumpu 4762 von 1 Händler(n) oder Hersteller(n) kaufen. Registrieren oder Anmelden um mehr Informationen erhalten.
PROSPECTOR
Finden Sie Lösungen, nicht nur Materialien.
Wenn Sie sich bei Prospector registrieren, können Sie unsere dynamischen Werkzeuge und Funktionen nutzen, um schnell Lösungen zu finden.
Noch heute registrieren