Outokumpu 1.4512
Type 12Cr-Ti stainless steel: EN 1.4512, AISI 409
Applications
- Automotive exhaust system parts: mufflers, pipes, catalytic converters, support parts.
- Constructional structures used in elevated temperatures.
Welding
- Conventional welding methods and filler materials applied to austenitic 300-series can be used.
- Titanium stabilized to be resistant against sensitization in Heat Affected Zone (HAZ).
- Shielding gases should be based on Ar/He, mixed with some oxygen to improve arc stability. Hydrogen and nitrogen must not be used.
- Heat input in welding should been kept in a minimum level.
Fabrication
- Grade 1.4512 can be formed using typical forming processes like folding, bending, drawing, etc.
- It has higher minimum proof strength than standard austenitic stainless steel grade 1.4301 / AISI 304 in combination with lower work hardening behavior.
- Due to the stabilization, the r-value is higher compared to the non-stabilized ferritic stainless steel such as 1.4016.
- These characteristics mean excellent deep-drawability and other forming related properties.
Corrosion resistance
- Outokumpu produces grade 1.4512 with a typical chromium content of 11,5 wt-% .
- Good corrosion resistance in moderate corrosive environment
- Grade 1.4512 is not susceptible to chloride induced stress corrosion cracking.
- The best material performance is reached usually with the help of adequate design, correct post-weld treatment and regular cleaning during use (if applicable).
一般的な属性
Prospectorで無料のアカウントを作成し、Outokumpu 1.4512のデータシート詳細すべてにアクセスします。そこで、物理、機械、硬度仕様に関するすべての情報をご覧ください
Technical Datasheet (English)
ドキュメントのダウンロード加工
Outokumpuの具体的な加工情報や、Steel - Wrought - Stainless - Ferriticジェネリックファミリーの一般情報をご確認いただけます。 登録 または サインイン 詳細情報を確認してください。
ご購入方法
1の販売業者や製造者からOutokumpu 1.4512を購入できます。 登録 または サインイン 詳細情報を確認してください。
PROSPECTOR
材料だけでなく、ソリューションも見つけることができます。
Prospectorにご登録いただくと、ダイナミックなツールおよび機能を活用して、迅速にソリューションを見つけることができます。
今すぐご登録ください