Nicrofer® 3220 HP - alloy 800 HP データシート

Wrought Nickel Alloy

Outokumpuで提供さ

Create your free Prospector account to view this complete product datasheet. A free account includes access to hundreds of thousands of detailed technical datasheets. 無料アカウントを作成しましょう
製品説明
Characteristics of Nicrofer 3220 HP - alloy 800 HP Nicrofer 3220 HP is an austenitic high-strength solid-solution nickel-iron-chromium alloy with controlled levels of carbon, aluminium, titanium, silicon and manganese and increased content of (Al + Ti).

A special solution anneal treatment (with grain sizes = 90 µm/ASTM No. 4) gives highest creep-rupture strength above 700 °C (1290 °F) due to the precipitation of TiC.

Below 700 °C (1290 °F), gamma prime (?´) precipitates combined with loss of ductility.

Nicrofer 3220 HP is characterized by:
  • excellent creep strength at temperature above 700 °C (1290 °F) However, for applications where frequent excursions to temperatures lower than 700 °C (1290 °F) during service cannot be excluded or parts of the material are permanently exposed to a temperature below 700 °C (1290 °F), the use of Nicrofer 3220 H is recommended.
  • good resistance to reducing, oxidizing and nitriding atmospheres and to atmospheres which alternate between reducing and oxidizing conditions
  • metallurgical stability in long-term application at high temperatures
一般  
供給体制 
  • 供給可能
供給可能地域 
  • アジア太平洋地域
  • アフリカ&中東
  • ラテンアメリカ
  • 北アメリカ
  • 欧州
Available Documents
Technical Datasheet (English)
Metals General
公称値
単位
 
Forms Available
 
 
Metal Type
 
 
Metals Type Analysis
公称値
単位
 
Type Analysis
     
Aluminum
%
 
Aluminum + Titanium
%
 
Carbon
%
 
Chromium
%
 
Copper
%
 
Iron (Balance)
%
 
Manganese
%
 
Nickel
%
 
Phosphorus
%
 
Silicon
%
 
Sulfur
%
 
Titanium
%
 
Metals Physical
公称値
単位
 
密度
lb/in³
 
Metals Mechanical
公称値
単位
 
Tensile Strength (Ultimate) (73°F)
ksi
 
Tensile Strength (Yield), 0.2% (73°F)
ksi
 
Tensile Elongation (Break) (73°F)
%
 
引張係数 (68°F)
ksi
 
Metals Thermal
公称値
単位
 
Mean Specific Heat (68°F)
Btu/lb/°F
 
Mean CTE (68 から 212°F)
in/in/°F
 
熱伝導性 (68°F)
Btu·in/hr/ft²/°F
 
Metals Electrical
公称値
単位
 
Electrical Resistivity (68°F)
ohms·cir·mil/ft
 
ノート
1一般的なプロパティ:これらは仕様として解釈されるものではありません。
 
UL および ULロゴはUL LLC © 2022の商標です。全権留保。
本データシートに表示されている情報は、UL Prospectorが材料の生産者より取得した情報です。UL Prospector は本データの精度を保証するために多大なる努力を払っています。しかしながら、UL Prospectorはデータ値に対してなんら責任を負わないものとし、最終的に材料を選択した場合に、材料サプライヤーとデータポイントを検証することを強くお奨めいたします。