Trímet EN AB-43200
Near-eutectic alloy with excellent castability properties and good resistance to hot tearing. Good machinability and excellent weldability.
Suitable applications:
For complicated thin-wall, pressure-tight, castings subjected to fatigue loading. High strength after heat treatment, but with limited corrosion resistance properties.
Heat treatment:
Solution heat treaded at 520-530°C for 3-6 hours followed by quenching in water and artificial ageing at 150-175°C for 15-5 hours
Propriétés générales
Consultez la fiche technique complète de Trímet EN AB-43200 en créant gratuitement votre compte Prospector. Vous y trouverez des informations exhaustives sur les propriétés physiques et mécaniques et sur la dureté
Technical Datasheet (English)
Télécharger le documentTraitement en cours
Find specific processing information for Trímet as well as general information for the Aluminum - Cast - Al-Si Alloy generic family. S’inscrire ou Connexion pour en savoir plus.
Où acheter
Vous pouvez acheter Trímet EN AB-43200 auprès de 1 distributeurs ou fabricants. S’inscrire ou Connexion pour en savoir plus.
PROSPECTOR
Trouvez des solutions, pas seulement des matériaux..
Avec Prospector, vous disposez d’outils et de fonctions dynamiques qui vous permettront de trouver des solutions au plus vite.
S’inscrire aujourd’hui