Sandmeyer Stainless Steel Alloy 17-4PH Fiche technique

Wrought Stainless Steel

Fourni par Sandmeyer Steel Company

Create your free Prospector account to view this complete product datasheet. A free account includes access to hundreds of thousands of detailed technical datasheets. Créez un compte gratuitement
Description du produit
Alloy 17-4PH (UNS S17400), Type 630, is a chromium-nickel-copper precipitation-hardening martensitic stainless steel with an addition of niobium. 17-4PH combines high strength and hardness with good corrosion resistance.

The alloy is furnished in the solution annealed condition (Condition A). It should not be used at temperatures above 572°F (300°C) or for cryogenic service. Optimal mechanical properties can be obtained by subjecting the alloy to age hardening heat treatments. Heat treatment in the 900°F (482°C) range produces the highest strength.

The corrosion resistance of Alloy 17-4PH is comparable to 304 stainless steel in most environments, and is generally superior to the 400 series stainless steels. It is used in applications where the combination of moderate corrosion resistance and unusually high strength are required.

Alloy 17-4PH can be easily welded and processed by standard shop fabrication practices. It is magnetic.

Applications
  • Aerospace — structural and parts
  • Biomedical — hand tools
  • Chemical Processing
  • Food Process Equipment
  • Gate Valves
  • Mechanical Components
  • Nuclear Waste Processing and Storage
  • Oil and Gas Production — foils, helicopter deck platforms, etc.
  • Pulp and Paper — paper mill equipment
Généralités  
État du matériau 
  • Commercial : actif
Disponibilité 
  • Afrique & Moyen-Orient
  • Amérique du Nord
  • Amérique latine
  • Asie Pacifique
  • Europe
Available Documents
Technical Datasheet (English)
Metals General
Valeur nominale
Unité
 
Applicable Specifications
 
 
Forms Available
 
 
Metal Type
 
 
Alloy Identification
 
 
Metals Type Analysis
Valeur nominale
Unité
 
Type Analysis
     
Carbon
%
 
Chromium
%
 
Copper
%
 
Iron (Balance)
%
 
Manganese
%
 
Nickel
%
 
Niobium + Tantalum
%
 
Phosphorus
%
 
Silicon
%
 
Sulfur
%
 
Metals Physical
Valeur nominale
Unité
 
Densité
lb/in³
 
Metals Mechanical
Valeur nominale
Unité
 
Tensile Strength (Ultimate) 2
ksi
 
Tensile Strength (Yield), 0.2% 2
ksi
 
Tensile Elongation (Break) 2
%
 
Reduction of Area 2
%
 
Dureté 2 (HRC-Scale)
 
 
Module de traction
ksi
 
Metals Thermal
Valeur nominale
Unité
 
Mean Specific Heat (68°F)
Btu/lb/°F
 
Mean CTE (70 à 801°F)
in/in/°F
 
Conductivité thermique (212°F)
Btu·in/hr/ft²/°F
 
Metals Electrical
Valeur nominale
Unité
 
Electrical Resistivity (75°F)
ohms·cir·mil/ft
 
Remarques
1Propriétés typiques : elles ne doivent pas être interprétées comme des spécifications.
2Condition: H900
 
UL et le logo UL sont des marques déposées de UL LLC © 2022. Tous droits réservés.
Les informations présentées sur cette fiche technique ont été obtenues par UL Prospector du producteur du matériau. UL Prospector met tout en œuvre pour garantir l’exactitude de ces données. Cependant, UL Prospector décline toute responsabilité pour les valeurs des données et recommande fortement de valider les différentes données auprès du fournisseur de matériau lors de la sélection finale du matériau.