Nicrofer® 3220 HP - alloy 800 HP Fiche technique

Wrought Nickel Alloy

Fourni par Outokumpu

Create your free Prospector account to view this complete product datasheet. A free account includes access to hundreds of thousands of detailed technical datasheets. Créez un compte gratuitement
Description du produit
Characteristics of Nicrofer 3220 HP - alloy 800 HP Nicrofer 3220 HP is an austenitic high-strength solid-solution nickel-iron-chromium alloy with controlled levels of carbon, aluminium, titanium, silicon and manganese and increased content of (Al + Ti).

A special solution anneal treatment (with grain sizes = 90 µm/ASTM No. 4) gives highest creep-rupture strength above 700 °C (1290 °F) due to the precipitation of TiC.

Below 700 °C (1290 °F), gamma prime (?´) precipitates combined with loss of ductility.

Nicrofer 3220 HP is characterized by:
  • excellent creep strength at temperature above 700 °C (1290 °F) However, for applications where frequent excursions to temperatures lower than 700 °C (1290 °F) during service cannot be excluded or parts of the material are permanently exposed to a temperature below 700 °C (1290 °F), the use of Nicrofer 3220 H is recommended.
  • good resistance to reducing, oxidizing and nitriding atmospheres and to atmospheres which alternate between reducing and oxidizing conditions
  • metallurgical stability in long-term application at high temperatures
Généralités  
État du matériau 
  • Commercial : actif
Disponibilité 
  • Afrique & Moyen-Orient
  • Amérique du Nord
  • Amérique latine
  • Asie Pacifique
  • Europe
Available Documents
Technical Datasheet (English)
Metals General
Valeur nominale
Unité
 
Forms Available
 
 
Metal Type
 
 
Metals Type Analysis
Valeur nominale
Unité
 
Type Analysis
     
Aluminum
%
 
Aluminum + Titanium
%
 
Carbon
%
 
Chromium
%
 
Copper
%
 
Iron (Balance)
%
 
Manganese
%
 
Nickel
%
 
Phosphorus
%
 
Silicon
%
 
Sulfur
%
 
Titanium
%
 
Metals Physical
Valeur nominale
Unité
 
Densité
lb/in³
 
Metals Mechanical
Valeur nominale
Unité
 
Tensile Strength (Ultimate) (73°F)
ksi
 
Tensile Strength (Yield), 0.2% (73°F)
ksi
 
Tensile Elongation (Break) (73°F)
%
 
Module de traction (68°F)
ksi
 
Metals Thermal
Valeur nominale
Unité
 
Mean Specific Heat (68°F)
Btu/lb/°F
 
Mean CTE (68 à 212°F)
in/in/°F
 
Conductivité thermique (68°F)
Btu·in/hr/ft²/°F
 
Metals Electrical
Valeur nominale
Unité
 
Electrical Resistivity (68°F)
ohms·cir·mil/ft
 
Remarques
1Propriétés typiques : elles ne doivent pas être interprétées comme des spécifications.
 
UL et le logo UL sont des marques déposées de UL LLC © 2021. Tous droits réservés.
Les informations présentées sur cette fiche technique ont été obtenues par UL Prospector du producteur du matériau. UL Prospector met tout en œuvre pour garantir l’exactitude de ces données. Cependant, UL Prospector décline toute responsabilité pour les valeurs des données et recommande fortement de valider les différentes données auprès du fournisseur de matériau lors de la sélection finale du matériau.