Outokumpu 4713
The two lower alloyed grades are best suited for temperatures between 550°C and 850°C, at which most HT austenitic stainless steels are prone to form brittle phases. The higher alloyed ones are applied at temperatures up to 1150°C and show excellent resistance against reducing sulphur attacks and molten metals.
Due to their ferritic structure, the ferritic steels show lower strength at temperatures exceeding 600°C, but are more resistant to thermal shocks than HT austenitic stainless steels. With the thermal conductivity higher and the thermal expansion lower than the respective values for austenitic steels, equal thermal shocks will result in lower thermal stresses in the ferritic material. In these terms, ferrites allow greater tolerances for design and operation.
All grades are included in the European Standard EN 10095 "Heat-resisting steels and nickel alloys".
4713 does not form brittle phases but should only be exposed to moderately corrosive atmospheres owing to its low chromium content.
Propriétés générales
Consultez la fiche technique complète de Outokumpu 4713 en créant gratuitement votre compte Prospector. Vous y trouverez des informations exhaustives sur les propriétés physiques et mécaniques et sur la dureté
Technical Datasheet (English)
Télécharger le documentTraitement en cours
Find specific processing information for Outokumpu as well as general information for the Steel - Wrought - Stainless - Ferritic generic family. S’inscrire ou Connexion pour en savoir plus.
Où acheter
Vous pouvez acheter Outokumpu 4713 auprès de 1 distributeurs ou fabricants. S’inscrire ou Connexion pour en savoir plus.
PROSPECTOR
Trouvez des solutions, pas seulement des matériaux..
Avec Prospector, vous disposez d’outils et de fonctions dynamiques qui vous permettront de trouver des solutions au plus vite.
S’inscrire aujourd’hui