Outokumpu 353 MA® Fiche technique

Cast Stainless Steel

Fourni par Outokumpu

Create your free Prospector account to view this complete product datasheet. A free account includes access to hundreds of thousands of detailed technical datasheets. Créez un compte gratuitement
Description du produit
A common feature of Outokumpu high temperature steels is that they are designed primarily for use at temperatures exceeding ~550°C, i.e. in the temperature range where creep strength as a rule is the dimensioning factor and where HT corrosion occurs. Optimising steels for high temperatures has meant that their resistance to aqueous corrosion has been limited. All steels are austenitic, resulting in relatively high creep strength values.

All steels except EN 1.4948 (i.e., all EN 1.48XX) are included in the European Standard EN 10095 "Heat-resisting steels and nickel alloys". EN 1.4948 is included in EN 10028-7 "Flat products made of steels for pressure purposes - Part 7: Stainless steel". All the above steel grades are also included in ASTM A240.

353 MA® is an alloy with a significantly higher nickel content than the other steels. Like 153 MA™ and 253 MA® it has increased contents of silicon and nitrogen, and is microalloyed with rare earth metals (REM). The maximum service temperature in air is 1150°C, but after service at temperatures below ~950°C there is a risk for reduced room temperature impact toughness.
Généralités  
État du matériau 
  • Commercial : actif
Disponibilité 
  • Afrique & Moyen-Orient
  • Amérique du Nord
  • Amérique latine
  • Asie Pacifique
  • Europe
Available Documents
Technical Datasheet (English)
Metals General
Valeur nominale
Unité
 
Applicable Specifications
 
 
Forms Available
 
 
Metal Type
 
 
Alloy Identification
 
 
Metals Type Analysis
Valeur nominale
Unité
 
Type Analysis
     
Carbon
%
 
Cerium
%
 
Chromium
%
 
Nickel
%
 
Nitrogen
%
 
Silicon
%
 
Metals Physical
Valeur nominale
Unité
 
Densité (68°F)
lb/in³
 
Metals Mechanical
Valeur nominale
Unité
 
Tensile Strength (Ultimate) (73°F)
ksi
 
Tensile Strength (Yield), 0.2% (73°F)
ksi
 
Tensile Elongation (Break) (73°F)
%
 
Dureté (HB-Scale, 73°F)
 
 
Module de traction (68°F)
ksi
 
Metals Thermal
Valeur nominale
Unité
 
Mean Specific Heat (68°F)
Btu/lb/°F
 
Mean CTE (68 à 212°F)
in/in/°F
 
Conductivité thermique (68°F)
Btu·in/hr/ft²/°F
 
Metals Electrical
Valeur nominale
Unité
 
Electrical Resistivity (68°F)
ohms·cir·mil/ft
 
Remarques
1Propriétés typiques : elles ne doivent pas être interprétées comme des spécifications.
 
UL et le logo UL sont des marques déposées de UL LLC © 2021. Tous droits réservés.
Les informations présentées sur cette fiche technique ont été obtenues par UL Prospector du producteur du matériau. UL Prospector met tout en œuvre pour garantir l’exactitude de ces données. Cependant, UL Prospector décline toute responsabilité pour les valeurs des données et recommande fortement de valider les différentes données auprès du fournisseur de matériau lors de la sélection finale du matériau.