Outokumpu 1.4318

Familia genérica: Steel - Wrought - Stainless - AusteniticSuministrado por: Outokumpu
Austenitic stainless steel
Type X2CrNiN18-7 stainless steel: EN 1.4318, AISI 301LN, low carbon, high nitrogen

Applications
  • Generally used for structural parts where high strength and toughness are needed beside a corrosion resistance similar to grade 1.4301 / AISI 304.
  • When hardened by cold working (surface finish 2H or TR), the strength and corrosion resistance of this steel grade steel is utilized in structural applications, like in transportation vehicles.
  • The combination between ductility and toughness is excellent even at low temperatures.

Welding
  • Weldability is good. The thermal expansion is 1,5-times larger compared with carbon steels.
  • Chromium and nickel contents of the filler metal have to match or to be higher than the composition of the base metal, e.g. type 19-9.
  • Cleaning the weld seam has a significant importance for corrosion resistance. Pickling is recommended.

Forming and machining
  • Work hardening is pronounced due to high work hardening rate and formation of martensite in the range of larger deformations.
  • Formability is good, thus forces needed and the elastic return is bigger compared with carbon steels and even when compared with grade 1.4301 / AISI 304.
  • Because of high ductility and work hardening it is recommended to use sharp cutting tools and an effective cooling and adequate feed of tool when machined.

Corrosion resistance
  • Corrosion resistance is comparable to grade 1.4301 / AISI 304.
  • Resistance to atmospheric corrosion is adequate for several applications. Special attention should be paid on surface finish and regular cleaning procedures in marine and industrial environments.
  • In chloride containing solutions pitting and crevice corrosion is possible depending on various parameters like chloride concentration, temperature, pH value, redox potential, crevice geometry and others.
  • When the temperature of chloride containing solutions exceeds 50°C and the construction is loaded, stress corrosion cracking is possible.
  • The best material performance is reached usually with the help of adequate design, correct post-weld treatment and regular cleaning during use (if applicable).
Propiedades generales

Acceda a los detalles completos de la hoja de datos de Outokumpu 1.4318 cuando cree su cuenta gratuita con Prospector. Encontrará información completa sobre especificaciones físicas, mecánicas y de dureza

Estado del material
Comercial: Activo
Documentos
description

Technical Datasheet (English)

Descargar documento
Disponibilidad
África y Oriente Medio, Asia-Pacífico, Europa, Latinoamérica, Norteamérica
Otras propiedades
Applicable Specifications, Metal Type, Alloy Identification, Type Analysis, Densidad, Tensile Strength (Ultimate), Tensile Strength (Yield), 0.2%, Tensile Elongation (Break), Mean CTE, Conductividad térmica
Access 10 properties in Metals. Create your free account or sign into Prospector.
Procesando

Encuentre información de procesamiento específica para Outokumpu, así como información general para la familia genérica de Steel - Wrought - Stainless - Austenitic. Registrarse o Iniciar sesión para obtener más información.

Dónde comprar

Puede comprar Outokumpu 1.4318 de 1 distribuidores o fabricantes. Registrarse o Iniciar sesión para obtener más información.

Inicio de sesión/Registro de Prospector
Características Premium

PROSPECTOR

Encuentre soluciones, no solo materiales.

Cuando se une a Prospector, aprovecha las herramientas y funciones dinámicas para encontrar soluciones rápidamente.

Regístrese hoy